A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: SU-8 spinning problems
SU-8 spinning problems
2002-03-15
Glen Landry
2002-03-15
[email protected]
2002-03-15
CLIF HAMEL
2002-03-15
Vic Kley
2002-03-15
Henry Yang
2002-03-15
[email protected]
wafer level vacuum packaging
2002-03-15
Krishna Kashyap
2002-03-15
CLIF HAMEL
SU-8 spinning problems
[email protected]
2002-03-15
> "200 rpm per second" ? Cliff???
>
> 200 rpm means 200 revolutions per minute.  Are you suggesting an
> acceleration or is it just a mistake?

When you program a newer model of spinner,
you can set the acceleration in addition to the rotational speed.
For example, an MTI Flexifab take takes the acceleration in krpm/s.

        --Kirt Williams Agilent Technologies

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Addison Engineering