Hello
Does anyone know how I would go about plating a nickel  corrosion coat on
stainless (to be used as a probe)?
I've heard that I must plate with copper first and then nickel.
Any information or source of information will be greatly appreciated.
Liz

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review