Dear David,
You can make a mask by getting a chrome blank - A virgin mask, they sell it with
resist on top. transfer the patern using you transparancy as a mask and etch the
chrome. If you need the pattern directly on glass, you can use an old mask or
glass wafer, spin coat it with resist, and pattern.


Shay Kaplan
Baoqing Li wrote:

> Hi,
>
> I have some transparent films with figures printed on it. Since the boss want
to save money, he won't make Cr-mask. He told me I can find a kind of glass
coated with photoresist and transfer the figures onto the glass. But the boss
has no ideal how to get the glass. Could you please tell me some information
about this kind of glass if you had used it?
>
> Thanks
>
> David Li
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation