Hi,
   Sounds like a job for SU8 from Microchem which I have seen 300 micron thick
or a photosensitive Polymide which can be up to 100 micron thick.  Bill
Moffat

-----Original Message-----
From: xiaohong [mailto:[email protected]]
Sent: Monday, April 22, 2002 3:05 PM
To: [email protected]
Subject: [mems-talk] pit coverage - with resist


 Hello all - I recently switched from Semiconductor to MEMS and have
never had to worry about the kind of topography I am seeing now - Anyone
have suggestions on a resist and program that could be used for 70um
deep pit coverage No small geometrics to resolve......


 Thanks Mike O' in Alberta
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing