If an etched part is not sufficient
please contact us.

Electroformed shadow masks micro-molds
and components routinely achieve sizes
and tolerances in the low micron level


-Mike

_______________
Mike Bigelow
Technical Sales

DRC - Metrigraphics
60 Concord Street
Wilmington, MA 01887   USA

Tel:  + (978) 658-6100  ext. 3063
Fax: + (978) 657-7765


-----Original Message-----
From: Klauder, Jr., Philip R. [mailto:[email protected]]
Sent: Friday, May 10, 2002 7:22 AM
To: '[email protected]'
Subject: RE: [mems-talk] Shadow masks


Try:
Photo Etch Technologies
978-805-5000
Lowell Mass

Phil Klauder
215-646-7400  x2151



-----Original Message-----
From: Stephen Bart [mailto:[email protected]]
Sent: Thursday, May 09, 2002 6:05 PM
To: [email protected]
Subject: [mems-talk] Shadow masks


I am looking for vendors who can construct a 6 in shadow mask with 1 mil
(25um) or better
resolution.

  Any suggestions?

--
*******************************************************************

Stephen F. Bart, Ph.D.

Technical Fellow, Core Technology Development

Coventor, Inc.
625 Mount Auburn Street
Cambridge, MA 02138  USA

*******************************************************************
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
Mentor Graphics Corporation
Harrick Plasma, Inc.