backside protection
Mac McReynolds
2002-06-06
You might look at UV release dicing tape.  It will resist strong HF
solutions, and after a flood UV exposure has very little "tack" or
stickiness

Mac McReynolds
R&D Manager
Caliper Technologies Corp.
605 Fairchild Drive
Mountain View, CA 94043-2234
Tel:  650-623-0710
Fax:  650-623-0521

> ----------
> From:         Roger Shile
> Reply To:     [email protected]
> Sent:         Wednesday, June 5, 2002 5:06 PM
> To:   [email protected]
> Subject:      [mems-talk] backside protection
>
> I am looking for a tape to put on the backside of 100 mm Si wafers to
> preserve
> the oxide on the back, while etching the front in buffered oxide etch.
>
> I have seen this done using dicing tape.  A coworker told me about
> something
> called "Yellow Tape" that came in circular pieces the same size as the
> wafer,
> apparently made for this purpose.  After use, the Yellow Tape was removed
> with
> acetone, which would be an advantage over peeling dicing tape from
> delicate
> substrates.
>
> Could someone refer me to a source for this Yellow Tape or suggest an
> alternative?
>
> Roger Shile
>
> "This email and any attachments may contain information that is
> confidential
> and proprietary information of Veeco Instruments Inc. and are intended
> only
> for the use of the addressee. Unauthorized use, distribution or copying is
> forbidden. If you have received this email in error, please notify the
> sender
> immediately by return email and delete all copies of this message and any
> attachments from your computer. Thank you."
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Nano-Master, Inc.
The Branford Group
Process Variations in Microsystems Manufacturing