PGMEA will attack the resist.  It is the base solvent for pretty much the
entire AZ series. It will dissolve both the exposed and unexposed regions of
the photoresist..

Best Regards,

Chad Brubaker



EV Group-Technology, Tel: (602) 437 9492 x 119, Fax: (602) 437 9435
E-mail: [email protected],  Web: www.EVGroup.com, 06/17/02

 -----Original Message-----
From:   LSWANG [mailto:[email protected]]
Sent:   Monday, June 17, 2002 1:34 AM
To:     [email protected]
Subject:        [mems-talk] SU8 developer ?

Hi,

Does anyone know if SU-8 developer such as PGMEA also
attacks AZ series ( after exposed ) Photoresist.
Thanks.

Lisen Wang
Yahoo! - Official partner of 2002 FIFA World Cup
http://fifaworldcup.yahoo.com
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
Harrick Plasma, Inc.
Mentor Graphics Corporation