MEMSnet Home: MEMS-Talk: Howcan I form parallel gold wires on thin layers ????
Howcan I form parallel gold wires on thin layers ????
2002-06-23
SHADY MORRIS
Howcan I form parallel gold wires on thin layers ????
SHADY MORRIS
2002-06-23
Can anyone inform me how to form a series of electric wires of gold for
example on a thin Polymide diaphragm (1.8 to 2.5 um) ?
Also I need to know how strong is the bond between these wires and the
diaphragm they are deposited on ?????

Plz reply as soon as Possible
                                                Thanks
                                            Shady Maurice

_________________________________________________________________
MSN Photos is the easiest way to share and print your photos:
http://photos.msn.com/support/worldwide.aspx

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics