MEMSnet Home: MEMS-Talk: Polyimide as a dielectric?
Polyimide as a dielectric?
2002-06-21
A H M Habib Ahsan
2002-06-21
[email protected]
2002-06-24
Rivas, Isabel
2002-06-25
White, Robert
Polyimide as a dielectric?
Rivas, Isabel
2002-06-24
Hello Habib,

Try with HD MicroSystems. Their web site is
www.hdmicrosystems.com/tech/polyimid.html.
I hope this information will help you.

Best regards,

> Isabel Rivas Guerrero
> CEIT, Microelectronic section
> Paseo de Manuel Lardizabal, 15.
> 20018 San Sebastian, Spain




-----Original Message-----
From: A H M Habib Ahsan [mailto:[email protected]]
Sent: 21 June 2002 06:33
To: [email protected]
Subject: [mems-talk] Polyimide as a dielectric?


Dear Sir/Madam:

Would you suggest me of some manufacturers who would be happy to tune up
some special polymides for me? My research work is seeking for some
polyimides to be used as a dielectric in a capciitive sensor.

I would be helped if you would redirect some name of them [manufacturers] to
me.

Thanks.

Habib [MecE, UofA, Canada]



---------------------------------
Post your ad for free now! Yahoo! Canada Personals
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Addison Engineering
MEMS Technology Review