MEMSnet Home: MEMS-Talk: doping effects in Si etching
doping effects in Si etching
2002-06-27
MARGOLLE Arnaud
2002-06-27
[email protected]
doping effects in Si etching
MARGOLLE Arnaud
2002-06-27
dear fellow ,
I need to delineate a PN junction  .(to etch more the doping zone than
undoped)
.Do you know something about the gas ,Ratio % ,sccm ;RF power, pressure
thanks you for your suggestions


        Arnaud Margolli
        DGA - Celar
        division DIRAC-TECN
        failure analysis -ECE Dep
        + 33  (0)  2 99  42 66 06

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.