Hi, there, use 1 M NaOH to dissolve the alumina.


shimin

pm72 wrote:

> I was wondering if there is a solution which can dissolve both Au and alumnina
> template. I need to dissolve the alumina template which is back sputtered
> with gold and then release nickel nanowires .Can any one give me the details?
>
> fabbi.
>
> PHANEENDRA MEDIDA
> Research Assistant
> Magnetic MEMS(Dr.Gary Friedman),
> Drexel University,
> Philadelphia PA 19104
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMS Technology Review
Addison Engineering
Process Variations in Microsystems Manufacturing