>       As an experiment, or unintentionally, has
> anyone encountered PLASMA CHARGE DAMAGE to their CMOS
> CHIPS (fully fabricated) when a MEMS Structure,
> along-side the CMOS Circuit, IS BEING RIE PLASMA ETCHED?
>
> I would appreciate some form of feedback. If the answer is yes, and a
> paper has been written about the experience, please let me know.

Phil,
charging damage is possible at all stages of the CMOS fabrication,
even on the finished chip, unless it's specifically designed
against it (reverse protection diodes).
One obvious source, the pulling of an electron current through
the substrate, is usually countered by magnetic electron confinement
and floating substrates.
Less obvious, but equally damaging, is electron/ion current uniformity
over the substrate - non-uniformity can lead to local charges which
discharge through your CMOS chip.

You'll find some literature and monitoring wafers at http://www.charm-2.com/
Also, you've got an expert inside BAE Systems. Talk to Dr. Russ Morgan
(Southampton Eng. Manager), and give him my regards ;-)

good luck
klaus

                        (TEEL)          Tokyo Electron Europe Limited
                                        PVD Process Support  (ex MRC)
Klaus Beschorner                                   Tel +49-7033-45683
Drosselweg 6                                       Fax +49-7033-45631
71120 Grafenau, Germany                       Mobile +49-174 315 7754

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Addison Engineering
Tanner EDA by Mentor Graphics