PDMS etching
Yen-Wen Lu
2002-07-10
Hi,
  Oxygen plasma etches PDMS very very slow while HF etches very fast.

yenwen

On Tue, 9 Jul 2002, Keyur Shah wrote:

> Hello everybody,
>
> I want to etch PDMS for my research work. Can anybody
> suggest me the ways to etch it? Is it possible to etch
> PDMS by using oxygen plasma? if yes, what is the etch
> rate?
>
> Thanking you all in anticipation,
>
> Keyur Shah
>
> =====
> Keyur Shah
> M.S(Chemical Engineering), Louisiana Tech University
> Research Assistant, Louisiana Tech University
> Apt#12, 106, South Homer Street,
> Ruston, Louisiana-71270,USA.
> phone no:318-513-9240
> Sign up for SBC Yahoo! Dial - First Month Free
> http://sbc.yahoo.com
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Addison Engineering