I am attempting to set up an anodic bonding tool that will be able to
uniformly bond 3" wafers.  At this point I am able to bond Corning 7070
Borosilicate glass to Si wafers but after the wafers have cooled there appears
to be minor defects in the glass surface in the form of 'pits'.  Each pit is
less than 50 um in diameter and hundreds are spread randomly throughout the
glass.  My setup is as follows:

Temp: 400 C
Voltage: 500-1200 V
Time: 1-5 mins
Electrodes: 304 Stainless Steel (lapped and polished on glass contact
surface)

Has anyone ever heard of this?  I have looked through some literature but
haven't found anything like this.

Any help is appreciated!
Brett Swope

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
MEMS Technology Review
Mentor Graphics Corporation