MEMSnet Home: MEMS-Talk: Help - - High optical refrative index polymer or UV glue
Help - - High optical refrative index polymer or UV glue
2002-07-31
Christopher Blanford
Help - - High optical refrative index polymer or UV glue
Christopher Blanford
2002-07-31
SU-8 has a refractive index of around 1.67 and meets your transparency
requirements.

Chris

> Would you please tell me where can I find a kind of
> polymer or UV glue, which has high optical refrative
> index (n=1.6~1.9) and has high transparent for h-line
> (for 405nm light, above 90%).
--
Christopher F. Blanford
Inorganic Chemistry Laboratory, South Parks Road, Oxford, OX1 3QR, UK
Phone: (44)/(0)-1865-282603; Fax: (44)/(0)-1865-272690
PGP keyID: 8D830BC9  http://pgp.mit.edu/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.