2002-09-06
Michael Yakimov
delamination of Au/Ni/Ge/Au layers in Citric acid solution etch
Michael Yakimov
2002-09-06
during annealing at 380C Au/Ge form an eutectic, which alloys to GaAs to
form a contact.. lower temperature anneals may produce SOME alloying.. from
my experience, even alloyed contact is easily attaced by GaAs etchants..
I've used photoresist to protect these contacts on backside of the wafer
during the etch..

Mike
> -----Original Message-----
> From: Parshant Kumar [SMTP:[email protected]]
> Sent: Thursday, September 05, 2002 1:30 PM
> To:   [email protected]
> Subject:      [mems-talk] delamination of Au/Ni/Ge/Au layers in Citric
> acid solution etch
>
> Hi All,
>
> I am working with the wet etch of GaAs in citric
> acid:Hydrogen peroxide::5:1. I am facing the problem that
> Electrode deposited as Au/Ni/Ge/Au layers start delaminated
> after 55-60 mintues of etching. However if we anneal the
> sample for 30 mintues at the 150 degree calcious, the
> effect is less.
>
> Any comment will be appericiated
>
> Thx
>
> Kumar
> Maryland MEMS Lab
> University of Maryland
> College Park-MD 20742
> Tel 301-405-0364
>
>
> __________________________________________________
> Do You Yahoo!?
> Yahoo! Finance - Get real-time stock quotes
> http://finance.yahoo.com
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
University Wafer
Addison Engineering