A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Sacrificial Layer for ZnO
Sacrificial Layer for ZnO
2002-09-23
Qihuo Wei
Sacrificial Layer for ZnO
Qihuo Wei
2002-09-23
Hi, All,

I am trying to find a sacrificial layer for ZnO film. It seems that etchant
for SiO2 or Si3N4 also attacks ZnO, does any one know how to etch SiO2 or
Si3N4 without attacking ZnO? Or any one knows there is another material
which can be used as sacrificial layer? Thanks a lot for your help.

Sincerely yours,

Qihuo Wei

Department of Mechanical & Aerospace Engineering
UCLA
Los Angeles, CA 90095
Tel: 310 825 7413
Fax: 310 206 2302




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Mentor Graphics Corporation