Do you want a Si wafer with build-in thermocouple (www.sensarray.com) or an
arsenic implanted silicon?
Mike

> -----Original Message-----
> From: Appel, Kim [SMTP:[email protected]]
> Sent: Tuesday, October 01, 2002 8:15 AM
> To:   [email protected]
> Subject:      [mems-talk] CALIBRATION SAMPLE for RTA
>
>
> Does anyone know where I could purchase a calibration wafer for an A.G.
> Assoc RTA?
> Regards,
> Kimberly Appel
> Picometrix, Inc
> 2925 Boardwalk Dr
> Ann Arbor Mi 48104
> (734) 998-4501 ext-5622
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
The Branford Group
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.