Fe contamination in KOH etching of silicon
2002-09-30
PEYRADE David
2002-10-08
Jamil El-Ali
Fe contamination in KOH etching of silicon
Jamil El-Ali
2002-10-08
Dear David

There was a paper on this issue at the Eurosensor 2000 conference from C.
Bergenstof Nielsen.

Regards,

Jamil El-Ali

-----Original Message-----
From: PEYRADE David [mailto:[email protected]]
Sent: 30. september 2002 16:53
To: '[email protected]'
Subject: [mems-talk] Fe contamination in KOH etching of silicon


Dear Mems Researchers,
I use KOH (prepared with prolabo powder) etching on Si (100) wafer, to
realize microreactors.
Here are the typical wet etching conditions : T=75°C, t=45min, KOH 40%M.
I do observe Fe particules (diameter < 500 nm) at the bottom of the
microreactors and suspect the KOH
product to introduce this pollution.
1) Does anyone have already observed this phenomenum ?
2) And do you have an idea to eliminate this pollution ?
Thanks a lot
 Best Regards,
David Peyrade




_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Addison Engineering
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing