MEMSnet Home: MEMS-Talk: Deep trench doping n+
Deep trench doping n+
2002-10-17
motocycle
2002-10-17
bille@npphotonics (Bill Eaton)
Deep trench doping n+
motocycle
2002-10-17
Hi:

   I  try to dope n+ into the Si trench.
   The trench opening is ~1um, and depth is 20um.
   I have no idea about this work.
   If anybody has this experience, please give me some suggestions.
   Thanks a lot.

   Mingching Wu