Au deposition on PDMS
2002-10-29
Changsoon Kim
Re: Au deposition on PDMS
2002-10-30
Bozhi Yang
2002-10-30
Dlee Li
2002-10-30
Bill Moffat
Re: Au deposition on PDMS
Bozhi Yang
2002-10-30
Hi, Changsoon,

I meet the similar problem and I ask people yesterday about it but have not
get a good answer.  If I get some answer I will let you know.  My problem
is to bond Au/or Aluminum to PDMS surface.  There is few refernence on such
stuff of Metal and PDMS.

Bozhi Yang
Scaife Hall 203, Dept. of Mechanical Engineering
Carnegie Mellon University
Pittsburgh, PA 15213
Phone: 412-268-3677(office)
email: [email protected]




--On Wednesday, October 30, 2002 11:48 AM +0900 Changsoon Kim
 wrote:

> Hello,
>
> How can the adhestion of Au to PDMS be increased?
> If you have any experience in using an adhesion
> promoter for this problem, please let me know.
>
> Thanks,
> Changsoon Kim
>



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics