MEMSnet Home: MEMS-Talk: Re: hydroxyl functional crosslinker
Re: hydroxyl functional crosslinker
2002-12-16
Jeff Classey
Re: hydroxyl functional crosslinker
Jeff Classey
2002-12-16
I'm not sure if your looking for an -OH in the polymer or just in the mix. Many
multifunctional polyols are used for epoxies and urethane
synthesis/crosslinking. For acrylate(free-radical) chemistry you can find
products from Sartomer with free -OH functionality . You can also use Darocur
1173 and/or Irgacure 184 from Ciba as photoinitiators, but these do not become
part of the matrix.

Jeff Classey
Senior Development Engineer
Digital Optics Corp.
9815 David Taylor Drive
Charlotte, NC 28262-2369
Ph: 704-887-3179
Fax: 704-887-3101


------------------------------

Date: Fri, 13 Dec 2002 23:49:52 -0800
From: "xu chenjie" 
To: [email protected]
Subject: [mems-talk] Is there such polymer?
Message-ID: 
Content-Type: text/plain; format=flowed
MIME-Version: 1.0
Precedence: list
Reply-To: General MEMS discussion 
Message: 5

I want to find some kind of polymer, which has hydroxyl in the linker. i
want to use it to reduce something that is dissolved in the polymer.





_________________________________________________________________


Jeff Classey
Senior Development Engineer
Digital Optics Corp.
9815 David Taylor Drive
Charlotte, NC 28262-2369
Ph: 704-887-3179
Fax: 704-887-3101


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
University Wafer
Nano-Master, Inc.