Dry film resist for greyscale lithography?
2002-12-16
Fred C Thomas III
Dry film resist for greyscale lithography?
Fred C Thomas III
2002-12-16
Is any one aware or had experience with using dry film photoresists for
greyscale lithographic applications. A dry film with fairly low contrast is
desired such that greyscale photomask features can be replicated in the dry
films thickness accurately and repeatably.

Thanks,

Fred


E-Business Card

Fred Thomas
Iomega Corporation
Building 8
1821 West Iomega Way
Roy, Utah 84067
USA

email: [email protected] 



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
Addison Engineering
Harrick Plasma, Inc.