MEMSnet Home: MEMS-Talk: Thin films on thick wafers
Thin films on thick wafers
2003-01-06
Shay Kaplan
Thin films on thick wafers
Shay Kaplan
2003-01-06
Hello Everyone,
We are looking for a thermal oxide / LPCVD nitride supplier that would
process 100mm dia, 1.5mm thick wafers.
Any lead is thankfully welcome,

Shay Kaplan