Happy New Year to ya'll!

I've been struggling for some time to find a source for  SIPOS -
Semi-Insulating-POlySilicon which is basically Oxygen rich polysilicon
 for use as a passivation layer.
I'd like to be able to test it on 4" wafers. Anyone have any ideas?

Thanks,

avi


Avi Laker
Teccor Electronics
972 756 8237   Office
214 439 6770   Pager



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
University Wafer