Dear all,
Have you experienced to use a Piranha cleaning step with GaAs wafer?
I want to know how much attack (surface roughening or etc) will be on
the GaAs wafer after the Piranha cleaning step.
Please, anyone would you let me know any information about that?
Thank you very much

Gunwoo Kim