2003-03-10
Sungjun Lee
Deposition of Gallium
Sungjun Lee
2003-03-10
Dear all :

I'm a graduate student and have no experience in handling Gallium.
I would like to do some experiment with pure Ga on a substrate.
After depositing Ga, I should take a surface image by atomic force microscopy.
The melting point of Gallium is 29C.

How can I deposit Ga(about 100nm) on metal substrate at my lab?
In addition, how can I handle it.

Please give me any comments about that.

Sungjun Lee / Physics student.



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
MEMS Technology Review
University Wafer