A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Deposition of Au into a microchannel
Deposition of Au into a microchannel
2003-03-10
[email protected]
2003-03-12
Likun Zhu
2003-03-11
Roger Shile
2003-03-11
[email protected]
Deposition of Au into a microchannel
Likun Zhu
2003-03-12
Try sputtering.

--- [email protected] wrote:
>
> Hi all,
>
> I am trying to deposit Au layer on the surface of a
> microchannel, both the
> walls and the bottom.  However, by evaporation the
> gold only deposits at the
> bottom surface;  the walls of the channel are not
> covered.  I am wondering if
> someone has experience solving this problem.
>
> Thanks alot!
>
> Zhiyu
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe
> or change your list
> options, visit
>
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS
> processing services.
> Visit us at http://www.memsnet.org/


__________________________________________________
Do you Yahoo!?
Yahoo! Web Hosting - establish your business online
http://webhosting.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Addison Engineering
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing