Hello,

I really thank you for your suggest. I have several question.

1. Is HF etchant Ok to Cr layer? wasn't there any reaction between Cr and HF
?
2. what was ratio of lateral/vertical etch rate?
3. what was etch rate to glass?
4. have you ever tried HF etching in 6:1 HF solution?

thank you,

SangHwui Lee
Ph.D candidate/MSE/NJIT
Microelectronics Research Center(MRC)
973-596-6368(O)
201-242-1486(H)


----Original Message Follows----
From: Robert D White 
Reply-To: General MEMS discussion 
To: [email protected]
Subject: [mems-talk] Re: Pyrex glass etching
Date: Thu, 06 Mar 2003 12:21:52 -0500

SangHwui,

I have been using a sputtered Cr/Au layer on my pyrex wafers as an
etch mask.  500 Ang Cr, 5000 Ang Au.  This can be patterned with
photolithography and Cr/Au wet etching.  Then strip the resist and go
into your pyrex etchant.  This stands up much better to HF than the
resist, but there is some undercut.  For your purposes, undercut might
not be a bad thing, since it will give a "slope" on the edge of your
etched region.  With long etches I observe significant roughening
of the pyrex surface, but I am etching much deeper (80 microns deep in
concentrated (49%) HF) than you are, so it might not be so bad for
you.

That's my experience.  If anyone has suggestions for how I might
reduce roughening or undercut in my pyrex etch process I would
appreciate the input.

Rob
--
Robert D. White
Graduate Student Research Assistant
Vibrations and Acoustics Lab, 2200 EECS
Mechanical Engineering
University of Michigan
Ann Arbor, MI 48109

(734)936-3824
[email protected]

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


_________________________________________________________________
Add photos to your e-mail with MSN 8. Get 2 months FREE*.
http://join.msn.com/?page=features/featuredemail


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics