MEMSnet Home: MEMS-Talk: how well does gold attach to zinc oxide
positive PR with no reaction with SU8
2003-03-24
gang hong
how well does gold attach to zinc oxide
2003-03-25
Shweta Humad
how well does gold attach to zinc oxide
Shweta Humad
2003-03-25

--
Shweta Humad
Hi all,

I had aluminum electrodes on a piezoelectric zinc oxide layer for my
devices. I was planning on using gold electrodes instead and was
wondering if anyone has had any experience with it. I'm not sure if
there is problem with gold maybe not attaching well to the zinc oxide.

Thank you!
Shweta Humad
[email protected]



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
University Wafer
Process Variations in Microsystems Manufacturing