Dear Mr. Yoo,
in our laboratory we have used the Epoxy Technology (www.epotek.com) products.
They sell epoxy resins fulfilling the highest biocompatibility standards (USP
VI).
In particular we have successfully used Epotek 353ND as adhesive, and EPOTEK
301-2 as encapsulant, for a silicon chemical microsystem.

Regards,
Lucia Beccai


Kyutae Yoo wrote:

> ------------------------------
>
> Message: 9
> Date: Mon, 14 Apr 2003 09:22:25 +0900
> From: "Kyutae Yoo" 
> Subject: [mems-talk] bio-compatible adhesive material
> To: 
> Message-ID: <003f01c3021b$ef46e840$0c91024b@LocalHost>
> Content-Type: text/plain;       charset="ks_c_5601-1987"
>
> Hello,
>
> I am looking for a bio-compatible adhesive material(glue) for wafer bonding.
> Does anyone know such material or have used it for wafer bonding?
> Thank you
>
> sincerely,
> ------------------------------------------------
> Kyutae Yoo, Ph.D.
>
> MEMS Lab
> Samsung Advanced Institute of Technology (SAIT)
> Tel(Office)   : +82-31-280-6948
> Fax(Office)  : +82-31-280-8277
> Tel(Mobile) : +82-11-345-5641
>
> ------------------------------

--
----------------------------------------------
Lucia Beccai, PhD
CRIM Lab
Polo Sant'Anna Valdera
Scuola Superiore Sant'Anna
Viale Rinaldo Piaggio 34 - 56025 -Pontedera (Pisa) - Italy
phone: +39 050 883 488
fax  +39 050 883 402
http://www-crim.sssup.it/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Addison Engineering