Yuebin Ning
Re: Grey Scale Mask
Yuebin Ning
2003-04-21
Han:

I believe DuPond Photomasks makes grey scale mask (http://www.photomask.com)

Yuebin Ning
Norcada Inc.

> Message: 4
> Date: Fri, 04 Apr 2003 14:13:42 +1000
> From: "Han  Chong" 
> Subject: [mems-talk] Grey scale mask
> To: 
> Message-ID: 
> Content-Type: text/plain; charset=US-ASCII
>
> Hi all,
>
> Does any one know where can I get a grey scale mask to be made?
>
> Thanks
>
> regards
>
> Han
>
> RMIT University


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Mentor Graphics Corporation
Addison Engineering
Tanner EDA by Mentor Graphics