i am geting a study on BaTiO3 PTC resistor devices..i have a electroding
problem.my electrodes shows high resistivity values.i need new but simple
technique that doesnt show oxidation problem!any (cheap)metal is ok for
me....Ag,Cu,Al...but how can i electrode on this PTC ceramic??
thanks a lot for your care!


_________________________________________________________________
MSN 8 with e-mail virus protection service: 2 months FREE*
http://join.msn.com/?page=features/virus


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
The Branford Group
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing