Bonding PDMS to SU-8
frank berisford
2003-04-29
Hello all,

Recently I've constructed some flow channels in SU-8 and would like to bond
PDMS to the SU-8.  I've had success in bonding PDMS to glass using an oxygen
plasma (50 Watts RF, 40sccm O2, 60mTorr, 5 minutes) and I tried the same recipe
for PDMS to SU-8 but it didn't work.

I was wondering if anyone else has tried this or could offer some suggestions.


Thank you,
Frank Berisford

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics