MEMSnet Home: MEMS-Talk: thermal effect on MUMPS
thermal effect on MUMPS
2003-05-05
weiwei2
2003-05-06
Cain, Mike
2003-05-06
Johnson, Stafford
thermal effect on MUMPS
weiwei2
2003-05-05
i did die attach of MUMPS die onto PCB using thermal cure epoxy at 150C. it
cause extra curling of MUMPS cantilever. how to solve this? is there any
literature on this?

LEOW
Universiti Teknologi Malaysia


reply