MEMSnet Home: MEMS-Talk: RE: Anisotropic Cu Wet etching
RE: Anisotropic Cu Wet etching
2003-05-06
HE,Han-Johnny
2003-05-07
Neal Ricks
2003-05-06
[email protected]
2003-05-07
David Nemeth
2003-05-09
HE,Han-Johnny
Materail for Thermal laternal actuator
2003-05-09
HE,Han-Johnny
2003-05-09
Kirt & Erika Zipf-Williams
RE: Anisotropic Cu Wet etching
Neal Ricks
2003-05-07
Johnny, I am having trouble finding on-line information about it, but there is a
company called McDermid Chemical that makes a Copper Etchant called "Fineline"
that might be worth checking out. Neal RicksShipley Co., LLC

"HE,Han-Johnny"  wrote:
Hi, David,

I am not using CMOS backend Damascene process for some limitation.

What I need is some good etchant of good selectivity for Cu over other
materials can be taken as Hard Mask(i.e. PhotoResist), most importantly,
of good functionality to give a good sidewall,(NO sideway etching) which
gives anisotropic etching.

Johnny
===========================================
Johnny H.HE, Ph.D. Candidate
Division of Electrical Engineering, Engineering
Department,Cambridge University,CB2 1PZ, UK
or Downing College, Cambridge, CB2 1DQ ,UK
Email: [email protected]
Tel:+44 1223 765199 Fax:+44 1223 332662
===========================================


----------------------------------------------------------------------

Message: 1
Date: Fri, 2 May 2003 10:38:33 -0400
From: "David Nemeth"
Subject: RE: [mems-talk] Anisotropic Cu Wet etching
To: "General MEMS discussion"
Message-ID:
Content-Type: text/plain; charset="us-ascii"

I don't have experience with this personally, but my understanding is
that CMOS processing of copper is done by forming grooves,
electroplating the copper, and polishing back to the tops of the
grooves. I don't know that a good anistropic etch exists for copper.

David Nemeth
Senior Engineer
Sophia Wireless, Inc.
14225-C Sullyfield Circle
Chantilly, VA
Ph: (703) 961-9573 x206
Fax:(703) 961-9576


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

---------------------------------
Do you Yahoo!?
The New Yahoo! Search - Faster. Easier. Bingo.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Mentor Graphics Corporation