MEMSnet Home: MEMS-Talk: soldering wafers with Ag top layers
soldering wafers with Ag top layers
2003-05-16
Micah Kemelman
soldering wafers with Ag top layers
Micah Kemelman
2003-05-16
hi,
I am trying to flip-chip bond two wafers that are covered with several layers,
the topmost of which is a thin (10-20 mu.m) Silver (Ag) layer. does anyone have
suggestions for a good leadless solder that can work?
thanks,
Micha