MEMSnet Home: MEMS-Talk: platinum on SU-8
platinum on SU-8
2003-07-01
Chen-Han Lee
2003-07-03
Kirt & Erika Zipf-Williams
2003-07-07
sokwon Paik
2003-07-07
Chen-Han Lee
2003-07-07
Mighty Platypus
2003-07-09
Chen-Han Lee
2003-07-07
Kirt & Erika Zipf-Williams
2003-07-01
[email protected]
2003-07-08
[email protected]
platinum on SU-8
Kirt & Erika Zipf-Williams
2003-07-03
> Good day everyone,
> I am a research student in U.K.
> Could anyone please tell me wome ways i can deposite platinum film on
SU-8?
> Any suggestions are welcomed.
> Thank you for your time.
> Chen-Han Lee

You can sputter or evaporate platinum.
Don't forget to use an adhesion layer.

    --Kirt Williams, Ph.D.   consultant


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Mentor Graphics Corporation