A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: AU electroplating solution
AU electroplating solution
2003-07-11
LSWANG
2003-07-14
transene
AU electroplating solution
transene
2003-07-14
Transene Company manufactures cyanide and sulfite based gold etchants.
The traditional cyanide etchant, SG-10, has been used in MEMS
applications.  Data sheets are available at www.transene.com.

Feel free to contact me if you would like additional information.

Christopher Christuk
Transene Company
10 Electronics Avenue
Danvers MA  01923
Tel:  978 777 7860
Fax:  978 739 5640
Email:  [email protected]

-----Original Message-----
From: LSWANG [mailto:[email protected]]
Sent: Friday, July 11, 2003 6:53 PM
To: [email protected]
Subject: [mems-talk] AU electroplating solution

Dear MEMS colleagues,
Can anyone give me some suggestion of what kind of Au
electroplating solution is widely used in MEMS
application, I have checked Technic 's website, they
have some kinds, but i don't know which one is better.
Thanks
Best
Lisen




Lisen Wang
Graduate student
University of California, Irvine

__________________________________
Do you Yahoo!?
SBC Yahoo! DSL - Now only $29.95 per month!
http://sbc.yahoo.com



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
University Wafer
Mentor Graphics Corporation