Graphite etchant?
2003-07-11
Amol Patil
2003-07-14
transene
Graphite etchant?
transene
2003-07-14
Graphite requires a dry etch process.

Christopher Christuk
Transene Company
10 Electronics Avenue
Danvers MA  01923
Tel:  978 777 7860
Fax:  978 739 5640
Email:  [email protected]

-----Original Message-----
From: Amol Patil [mailto:[email protected]]
Sent: Friday, July 11, 2003 6:58 PM
To: [email protected]
Subject: [mems-talk] Graphite etchant?

Does anyone know of method and liquids for etching graphite ? I did try
the piranha etch at 70 degrees  but I am not getting conclusive results.
Does piranha etch graphite?

Thanks for your help
Amol Patil


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
The Branford Group
University Wafer