MEMSnet Home: MEMS-Talk: Glass-Glass thermal fusion bonding
Glass-Glass thermal fusion bonding
2003-08-11
Balaji Srinivasan Venkatesh
2003-08-12
Brubaker Chad
2003-08-28
Sooje Cho
Glass-Glass thermal fusion bonding
Sooje Cho
2003-08-28
The glasses are bonded generally at elevated temperature.
The temperature is varied by the glass composition.
General sodalime glass is bonded at the temperature of 500C-600C.
The surface of glass must be polished finely to get good bonding.
Vacuum annealing(heating) has good effects in case your glass is not
polished.

Sooje Cho from MEMSware



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Tanner EDA by Mentor Graphics
The Branford Group
Mentor Graphics Corporation