Underetch Measurement
2003-09-04
Tom Fan
2003-09-04
[email protected]
2003-09-05
Jason Viotty
Underetch Measurement
[email protected]
2003-09-04
A standard Dektak or other profilometer will give you accurate depth
measurements depending on the width of the feature you are trying to measure.
The larger the pitch the better for measurement accuracy. Bob Henderson

reply