how to buy a CO2 supercritical dryer
2003-09-06
GuyHaché
2003-09-07
Christopher Blanford
how to buy a CO2 supercritical dryer
Christopher Blanford
2003-09-07
Dear Guy

I have had a good experience with our Emitech K850 CPD. The staff were
knowledgeable and the service has been very good.

Chris

On Saturday, September 6, 2003, at 08:21 PM, Guy Haché wrote:

> I am searching for some information about CO2 supercritical dryer.  I
> would like
> some suggestions about which compagny I should approach to buy a CO2
> supercritical dryer or which I should not! If you also know some
> publications
> that cited  a particular CO2 supercritical dryer or if you use (or
> sell) one,
> please contact me.

--
Christopher F. Blanford
Inorganic Chemistry Laboratory, South Parks Road, Oxford, OX1 3QR, UK
Phone: +44 (0)1865 282603; Fax: +44 (0)1865 272690
PGP keyID: 8D830BC9  http://pgp.mit.edu/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation