S1805 solvent
Rob Hardman
2003-09-10
Hi Laurent,



Yes, the solvent is propylene glycol monomethyl ether acetate. It is sold by
Shipley (Also by us at MicroChem as their distributor) in the U.S. as Type P
Thinner. However, just to make clear things muddy, it is also sold as "EC
Solvent" by Shipley in Europe. The products are identical. Just be careful
because the EC Solvent 11 product sold in the U.S. is NOT THE SAME. It is ethyl
lactate.

Hope that 's no too much information!

Very Best Regards,
Rob Hardman
617-965-5511 ext.313
[email protected]

www.microchem.com




Date: Mon, 08 Sep 2003 16:03:58 +0000

From: "laurent gangloff" 

Subject: [mems-talk] shipley 1805 solvent?

To: [email protected]

Message-ID: 

Content-Type: text/plain; charset=iso-8859-1; format=flowed

Hi all,

Could anyone tell me what is the solvent use in the 1805 resist from

shipley?

Thanks.

_________________________________________________________________

Hotmail : un compte GRATUIT qui vous suit partout et tout le temps !

http://g.msn.fr/FR1000/9493

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Nano-Master, Inc.
Tanner EDA by Mentor Graphics