Thank you for telling me your experience.
Greetings
Stefan

-----Original Message-----
From: Xu Zhu [mailto:[email protected]]
Sent: Montag, 15. September 2003 19:25
To: General MEMS discussion
Subject: RE: [mems-talk] SF6 Glas etching


Stefan,

My experience was: running a long etch with Ar will change your silicon
etch process, especially when running at low pressure and high power.


Xu Zhu

-----Original Message-----
From: Jim Beall [mailto:[email protected]]
Sent: Monday, September 15, 2003 10:23 AM
To: General MEMS discussion
Subject: Re: [mems-talk] SF6 Glas etching

Stefan -

I wonder if you ever received any useful information in response to
this inquiry?

We also have an STS ASE system and were told to never do anything
else so as to not disturb the chamber chemistry, but I wonder how
critical this really is.

Thanks,

Jim

>Dear colleagues
>>From the publication of Ichiki et al. Thin Solid Films 435 (2003)
62-68
>I learned that glas
>etching with SF6 and Ar works quiet well. When we bought 4 years ago a
>ICP system (STS) for Si deep etching and a RIE system for glas (resp
>SiO2, Si3N4)
etching
>we were told from STS not to do
>both processes in the same chamber because of reproducibility. Does
>anyone has experience in running glas etch (SF6/Ar) and silicon deep
>etching on the same ICP system. Do I contaminate the si deep etching
>chamber by glass etching
>or is it possible to clean up the system without open it (no mechanical
>clean)?
>
>Thanks for response.
>Greetings
>Stefan

--

  - Jim Beall 303-497-5989
    [email protected]



_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Mentor Graphics Corporation
Addison Engineering
Tanner EDA by Mentor Graphics