MEMSnet Home: MEMS-Talk: RE: SF6 Glas etching (Blunier, Stefan)
RE: SF6 Glas etching (Blunier, Stefan)
2003-09-17
Rebello, Keith J.
RE: SF6 Glas etching (Blunier, Stefan)
Rebello, Keith J.
2003-09-17
Stefan,
I have seen a decrease in Si etch rates after Ar enhanced etching/milling.
We use a dedicated ICP chamber for silicon and another chamber for other
materials.
Cheers,
Keith