MEMSnet Home: MEMS-Talk: Finding selective etchant for W and Mo
Finding selective etchant for W and Mo
2003-09-23
sajid
Finding selective etchant for W and Mo
sajid
2003-09-23
Hi Lee,

Hydrogen peroxide H2O2 might be a solution that etches W and Mo
selectively over Au and Ti. I however do not know the selectivity.

Sajid