A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Does molten Indium wet SiO2 surface?
Does molten Indium wet SiO2 surface?
2003-09-25
Yuanbo Zhang
2003-09-25
Kirt & Erika Zipf-Williams
Does molten Indium wet SiO2 surface?
Yuanbo Zhang
2003-09-25
Hi all,

I am trying to thermally evaporate ~30nm Indium film onto SiO2
substrate, then heat it up
  to the melting temperature of Indium. Does anyone know if Indium wets
SiO2 surface?
  If it does NOT wet, how is the adhesion between Indium and SiO2? If it
does wet, what
kind of substrate should I use to get a non-wetting contact?

Any suggestions would be greatly appreciated.

Yuanbo Zhang
Dept. of Physics, Columbia University
538 West 120th St., PUPIN 704
New York, NY 10027
Phone: (212)8540393
Fax: (212)8540392


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Mentor Graphics Corporation
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing