MEMSnet Home: MEMS-Talk: photoresist remove
photoresist remove
2003-10-02
Yilei Zhang
2003-10-03
Eric Miller
2003-10-03
Bill Moffat
2003-10-03
Michael D Martin
photoresist remove
Yilei Zhang
2003-10-02
Dear Members:
I have some samples with photoresist (AZ5209) coating for a long time, now i
cannot
remove it by aceton, stripper, or ultrasonic cleaner. Can anyone give me some
suggestions? Thanks.

Regards,
Yilei Zhang










reply