A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: How to separate a silicon chip from a pyrex glas
How to separate a silicon chip from a pyrex glas
2003-10-17
Schlienger, Joel P.
2003-10-20
Tomblin, Graham (OH32)
2003-10-21
Joel Schlienger
2003-10-21
Rich Rosenblum
How to separate a silicon chip from a pyrex glas
Tomblin, Graham (OH32)
2003-10-20
Joel
You may be able to dice off the pyrex using a diamond saw or perhaps drilling a
hole using ultrasonic milling or
sanblasting with a fine nozzle.
Either way you have to be careful not to damage the sensor chip.
Alternatively find someone who will give you a a gage prssure chip, try silicon
micro structures in milpitas California
Graham

-----Original Message-----
From: Schlienger, Joel P. [mailto:[email protected]]
Sent: Friday, October 17, 2003 2:45 PM
To: [email protected]
Subject: [mems-talk] How to separate a silicon chip from a pyrex glas


Does anybody has the experience on how to separate a pressure silicon chip from
the pyrex support glas. I have a chip
that is mounted by anodic bonding on the pyrex but need to remove it in order to
use the pressor sensor in gauge
conditions.

Thanks for any comments on that.

Joel

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
The Branford Group
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.